소결부품 소결부품

소결부품





MATERIALS FOR OIL IMPREGNATED BEARINGS


MATERIALS

DENSITY(g/cm³)

APPLICATIONS

CHARACTERISTICS

Cu-Sn

6.0-6.8

Micro motors

Precise mini components

Cu-Sn-C

6.8-7.5

Audio Equipment

Pb(C) enhance shaft/Bearing lubrication

Cu · Sn · MoS₂

6.4-7.2

Office equipment

Solid Lubricants, durable materials

Fe 係

5.8-7.0

Home appliances

Customer electronics

Medium & High load



MATERIALS FOR STRUCTURAL PARTS


MATERIALS

DENSITY(g/cm³)

HARDNESS(HRB)

T.S(kg/mm²)

CHARACTERISTICS

Fe

6.2 - 7.0

10 – 50

10 – 25

Pure lron

Fe · Cu

6.2 - 7.0

20 – 60

10 – 35

Copper-alloy steel

Fe · Cu · C

6.2 - 7.0

30 – 70

20 – 60

Copper-carbon steel

Fe · Cu · C · Ni

6.6 - 7.0

40 – 65

30 – 45

Nickel-alloy steel

Fe · Cu · C · Ni · Mo

7.0 - 7.4

60 - 100

60 - 75

Alloyed steel



SOFT MAGNETIC PROPERTIES OF SINTERED MATERIAL


MATERIALS

B (C)

Br (C)

Hc (Oe)

PERMEABILITY

APPLICATIONS

Permalloy

6,000

1,000

0.9

7400

Yokes

13,000

8,000

0.4

1,000

Solenoid, Yokes 

STS430

11,000

7,500

1.4

3,000

Solenoids



GRADES OF TUNGSTEN HEAVY ALLOY


GRADE

CS90

CS92.5

CS95

CS97

Composition[wt%]

90W

92.5W

95W

97W

Density[g/cm³]

16.8 ~ 17.2

17.3 ~ 17.7

17.8 ~ 18.2

18.3 ~ 18.5

Hardness[HRC]

25 ~ 34

27~ 35

28~ 36

30~ 37

Tensile Strength[N/mm²]

~ 1000

~ 950

~ 800

~ 700

Electrical Conductivity[%IACS]

10 ~ 15

13 ~ 15

13 ~ 16

14 ~ 17

Coefficient of Thermal Expansion[x 10⁴ K]

4.6 ~ 5.4

4.4 ~ 4.6

4.4 ~ 4.6

4.4 ~ 4.5

Elongation[%]

~ 20

~ 10

~ 7

~ 5